Superalloy AAAC Cable/All Aluminum Alloy Conductor 25mm 35mm 40mm 50mm 150mm 170mm 300mm
Superalloy AAAC Cable/All Aluminum Alloy Conductor 25mm 35mm 40mm 50mm 150mm 170mm 300mm image
Get Latest Price Request a quote
Quick Details
Product Details
superalloy AAAC cable/All Aluminum Alloy Conductor 25MM 35MM 40MM 50MM 150MM 170MM 300MM
DESCRIPTION
The conductor consists of Aluminum Magnesium-Silicon alloy wires stranded in successive layers in opposite direction and the outer layer is right hand direction Z. Natural grease may be applied between the layers of AAAC except the outer layer.
STANDARD
Construction as per ASTMB399,DIN48201,BS EN50182,IEC61089,CSA49
APPLICATION :
AAAC bare conductors are used for primay and secondary overhead power transmission lines haveing long spans and high resistance to corrosion .
Product photo :
CERTIFICATE:
| Nominal Area (mm2) |
Cross Section (mm2) |
Stranding and wires Dia. (mm) |
Overall Dia. (mm) |
Weight (kg/km) |
Rated strength (kN) |
Max.D.C. Resistance (Ω/km,20ºC) |
| BOX | 18.8 | 7/1.85 | 5.55 | 51.4 | 5.55 | 1.7480 |
| ACACIA | 23.8 | 7/2.08 | 6.24 | 64.9 | 7.02 | 1.3828 |
| ALMOND | 30.1 | 7/2.34 | 7.02 | 82.2 | 8.88 | 1.0926 |
| CEDAR | 35.5 | 7/2.54 | 7.62 | 96.8 | 10.46 | 0.9273 |
| DEODAR | 42.2 | 7/2.77 | 8.31 | 115.2 | 12.44 | 0.7797 |
| FIR | 47.8 | 7/2.95 | 8.85 | 130.6 | 14.11 | 0.6875 |
| HAZEL | 59.9 | 7/3.30 | 9.90 | 163.4 | 17.66 | 0.5494 |
| PINE | 71.6 | 7/3.61 | 10.8 | 195.6 | 21.14 | 0.4591 |
| HOLLY | 84.1 | 7/3.91 | 11.7 | 229.5 | 24.79 | 0.3913 |
| WILLOW | 89.7 | 7/4.04 | 12.1 | 245.0 | 26.47 | 0.3665 |
| OAK | 118.9 | 7/4.65 | 14.0 | 324.5 | 35.07 | 0.2767 |
| MULBERRY | 150.9 | 19/3.18 | 15.9 | 414.3 | 44.52 | 0.2192 |
| ASH | 180.7 | 19/3.48 | 17.4 | 496.1 | 53.31 | 0.1830 |
| ELM | 211.0 | 19/3.76 | 18.8 | 579.2 | 62.24 | 0.1568 |
| POPLAR | 239.4 | 37/2.87 | 20.1 | 659.4 | 70.61 | 0.1387 |
| SYCAMORE | 303.2 | 37/3.23 | 22.6 | 835.2 | 89.40 | 0.1095 |
| UPAS | 362.1 | 37/3.53 | 24.7 | 997.5 | 106.82 | 0.0917 |
| YEW | 479.0 | 37/4.06 | 28.4 | 1319.6 | 141.31 | 0.0693 |
| TOTARA | 498.1 | 37/4.14 | 29.0 | 1372.1 | 146.93 | 0.0666 |
| RUBUS | 586.9 | 61/3.50 | 31.5 | 1622.0 | 173.13 | 0.0567 |
| SORBUS | 659.4 | 61/3.71 | 33.4 | 1822.5 | 194.53 | 0.0505 |
| ARAUCARIA | 821.1 | 61/4.14 | 37.3 | 2269.4 | 242.24 | 0.0406 |
| REDWOOD | 996.2 | 61/4.56 | 41.0 | 2753.2 | 293.88 | 0.0334 |
| Code name |
Cross Section (mm2) |
Stranding and wires Dia. (in) |
Overall Dia. (mm) |
Weight (1b/1000ft) |
Rated strength (kN) |
Max.D.C. Resistance (Ω/km,20ºC) |
| Akron | 15.5 | 7/0.0661 | 5.04 | 28.52 | 4.92 | 2.159 |
| Alton | 24.7 | 7/0.0834 | 6.36 | 45.40 | 7.83 | 1.356 |
| Ames | 39.2 | 7/0.1052 | 8.01 | 72.24 | 12.4 | 0.8547 |
| Azusa | 62.4 | 7/0.1327 | 10.11 | 114.9 | 18.9 | 0.5365 |
| Anaheim | 78.6 | 7/0.1490 | 11.34 | 144.9 | 23.8 | 0.4264 |
| Amherst | 99.3 | 7/0.1672 | 12.75 | 182.5 | 30.0 | 0.3373 |
| Alliance | 125 | 7/0.1878 | 14.31 | 230.2 | 37.8 | 0.2678 |
| Butte | 159 | 19/0.1283 | 16.3 | 291.6 | 46.5 | 0.2112 |
| Canton | 200 | 19/0.1441 | 18.3 | 367.9 | 58.6 | 0.1676 |
| Cairo | 236 | 19/0.1565 | 19.9 | 433.9 | 69.2 | 0.1417 |
| Darien | 284 | 19/0.1716 | 21.8 | 521.7 | 83.1 | 0.1181 |
| Elgin | 331 | 19/0.1853 | 23.55 | 608.3 | 97.0 | 0.1012 |
| Flint | 375 | 37/0.1415 | 25.13 | 690.8 | 107 | 0.08944 |
| Greeley | 470 | 37/0.1583 | 28.14 | 864.6 | 135 | 0.07133 |
We are China Superalloy AAAC Cable/All Aluminum Alloy Conductor 25mm 35mm 40mm 50mm 150mm 170mm 300mm manufacture and supplier,You can get more details with Email,you will get cheap price or factory price.
Get Latest Price Request a quote
Popular Electric Cable Products
5kv 3X1/0AWG Epr Insulated Copper Tape Shield Mc-Hl Mv-105 Power Cable
H07V-U H07V-R H07V-K 16mm2 PVC Insulated Electric Wire Cable
H05z-K, Electric Wire, 300/500 V, Cu/Lszh, Low Smoke Halogen Free Cable (HD 22.9)
No1 450/750 V H07rn-F Epr Rubber Insulated PVC Sheath Cable 1.5mm2 Control Cable Electric Wire
Low Voltage Single Core Three Cores Foure Cores PVC Insulated PVC Sheathed Electrical Cable
1*10AWG+10AWG Copper or Aluminium Conductor Concentric Electric Cable
Popular Flexible Cable Products
PVC Insulated Flexible Copper Electric Cable PVC Shielded Wire Rvvp
H07z-U H07z-R H07z-K Halogen Free Single Core Wire Lsoh PVC Flexible Cable
Indoor and Outdoor Rubber Jacket Power Cable
1.5/2.5mm2 Copper Flexible Cable for 300/500V
Thw House Wire Builing Wire Electric Cable Wire
Flexible Silicone Cable Manufacturer Rubber Welding Cable
Popular Power Cable Products
BS Standard Tiger Aluminum Electric Wire Steel Reinforced ACSR Conductor
33 Kv 1 Core 500 mm Sq XLPE Underground Copper Cable Awa
Copper Conductor PVC Insulated Marine Power Cable
Manufacturer 150m/Spool Canada Wire Electric Power Copper UL Cable Nmd90 Nmd 90 Nmwu
4 Core 25mm2 35mm2 Yjv Copper XLPE Insulation Underground Power Cable
UL CSA List Electric Power Urd Cable #1/0 AWG 15kv Rubber Epr 133% Cu Mv-105
Popular zzjinshui Products
ACSR 120/20 and Caa Conductor ACSR Aluminum Conductor Steel Reiforced
ACSR Copper Wire Aluminum Conductor Power Cable
Low Voltage Copper Conductor 4 Core XLPE Armoured Cable
Triplex Service Drop 0.6/1kv Cable
ABC Overhead XLPE Insulated Cable AWG 6 Chola
Tags: Electric Cable, Flexible Cable, Power Cable, zzjinshui